Figure 4.

Fiber analysis: electrospun nylon. SEM images indicated that fibers were produced under all conditions assayed. Fibers electrospun from the 60 mg/ml solutions were smaller than all other treatment groups (P < 0.05) and fibers from 80 mg/ml solutions were smaller than fibers in the 140 mg/ml solutions (P < 0.05).

Manis et al. Journal of Biological Engineering 2007 1:2   doi:10.1186/1754-1611-1-2